Abstract
This paper explores the atomic layer deposition (ALD) of indium oxide (In2O3) films using cyclopentadienyl indium (InCp) and combinations of both molecular oxygen and water as the co-reactants. When either O2 or H2O were used individually as the oxygen source the In2O3 growth was negligible over the temperature range 100−250 °C. However, when oxygen and water were used in combination either as a simultaneous exposure or supplied sequentially, In2O3 films were deposited at growth rates of 1.0−1.6 A/cycle over the full range of deposition temperatures. In situ quadrupole mass spectrometry and quartz crystal microbalance measurements revealed that water serves the function of releasing ligands from the surface while oxygen performs the role of oxidizing the indium. Since both processes are necessary for sustained growth, both O2 and H2O are required for the In2O3 ALD. The electrical resistivity, mobility, and carrier concentration of the In2O3 films varied dramatically with both the deposition temperature an...
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.