Abstract

The hearth is a crucial region of the blast furnace, since the life of its refractory may be decisive for the campaign length of the furnace. Excessive growth of skull on the hearth wall and bottom, in turn, reduces the inner volume of the hearth, causes drainage and other problems that limit productivity, and has a negative effect on hot metal temperature and chemistry. A set of indicators that reflect the internal state of the hearth has been developed. The motivation for the indicators is outlined and their application to hearth state detection is illustrated with several examples from the operation of two Finnish blast furnaces.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.