Abstract
Molecular dynamics (MD) simulation was used to systemically investigate the nanoindentation process of GaN. Different loading orientations and indenter radii were simulated and studied. In this work, the variation of stress propagation, particle movement and evolution of dislocations were discussed in detail. The size of the indenter has an important influence on the occurrence of plastic deformation. As the size of the indenter increases, the critical load of plastic deformation increases and the critical shear strain decreases. In addition, the nucleation and propagation of dislocations during initial plastic deformation is always along the low-strain region. The propagation of dislocation varied in a similar trend as the atomic displacement and atomic stress. The nano-hardness value of GaN during the indentation process was significantly affected by the size effect. Among them, the polar plane of GaN has higher hardness and the dislocations were pinned to the sample surface, which would not slip and propagate into the sample. However, during the indentation process perpendicular to the a-plane and m-plane, there were two types of dislocations in the sample, which were nailed to the surface or propagated to the inside of the sample.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.