Abstract
Bone regeneration can be accelerated by localized delivery of appropriate growth factors/biomolecules. Localized delivery can be achieved by a 2-level system: (i) incorporation of biomolecules within biodegradable particulate carriers (nanoparticles), and (ii) inclusion of such particulate carriers (nanoparticles) into suitable porous scaffolds. In this study, freeze-dried porous chitosan–gelatin scaffolds (CH–G: 1:2 ratio by weight) were embedded with various amounts of poly(lactide-co-glycolide) (PLGA) nanoparticles, precisely 16.6%, 33.3% and 66.6% (respect to CH–G weight). Scaffolds loaded with PLGA nanoparticles were subjected to physico-mechanical and biological characterizations including morphological analysis, swelling and dissolution tests, mechanical compression tests and cell viability tests. Results showed that incorporation of PLGA nanoparticles into porous crosslinked CH–G scaffolds: (i) changed the micro-architecture of the scaffolds in terms of mean pore diameter and pore size distribution, (ii) reduced the dissolution degree of the scaffolds, and (iii) increased the compressive modulus. On the other hand, the water uptake behavior of CH–G scaffolds containing PLGA nanoparticles significantly decreased. The incorporation of PLGA nanoparticles did not affect the biocompatibility of CH–G scaffolds.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of the Mechanical Behavior of Biomedical Materials
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.