Abstract
The article presents and characterises Incoloy 800HT iron-based superalloy in terms of: chemical composition, heat treatment, microstructure and properties, in its delivery condition. This material is commonly used in process lines in the petrochemical industry, e.g. into components called ‘pigtails’.