We examined the effects of various ions on the mineralization of dentin matrix in vitro. Demineralized dentin matrix was incubated in a metastable calcium phosphate solution with or without silicate, fluoride, calcium, phosphate, magnesium or silver. Insoluble dentin matrix induced mineral formation after incubation for 10.2 h in the metastable solution without added ions. Silicate at 5 µM and fluoride at 40 µM significantly reduced the mineral induction time. At least 200 µM calcium or 100 µM phosphate was required to promote mineral induction. Conversely, magnesium and silver concentrations as low as 10 and 2 µM inhibited mineral induction. The mineral induced by each sample after incubation for 24 h was identified by its X-ray diffraction pattern as apatite. We concluded that silicate is a stronger inducer of remineralization of dentin matrix than fluoride, calcium or phosphate, and that magnesium and silver inhibit the induction of remineralization of dentin matrix.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call