Abstract
Magnesium and its alloys are biodegradable materials with great potential for biomedical development; however, their high rate of degradation in biological environments limits the widespread application of these materials. In order to improve the corrosion resistance of magnesium alloy, a functional calcium phosphate coating was prepared on Mg-3Zn-0.5Zr-0.5Sr alloy by microarc oxidation (MAO) combined with chemical deposition of fluoridated hydroxyapatite (FHA). A dense calcium-phosphorus coating 6 μm thick composed of needle-shaped fluoridated hydroxyapatite formed on the surface of the MAO layer. The MAO-FHA coating exhibited good mineralization ability to induce hydroxyapatite deposition on its surface during degradation testing in simulated bodily fluids.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.