The aim of this study was to investigate the in vitro and in vivo properties and degradation of (1) self-reinforced (SR) lactide copolymer, P(L/DL)LA 70:30, and (2) SR composites of the same polylactide and bioactive glass 13-93. The following three polymer and polymer-bioactive glass samples were studied: SR-PLA70, SR-PLA70 + BaG15s, and SR-PLA70 + BaG20c. In vitro behavior was studied in a phosphate-buffered saline for 87 weeks at 37 degrees +/- 1 degrees C and a pH of 7.4 +/- 0.2. In vivo behavior was studied by implanting the rods in the dorsal subcutaneous tissue of rats (SR-PLA70 + BaG20c) or rabbits (SR-PLA70 and SR-PLA70 + BaG15s) for 48 weeks. The degradation of the specimens was evaluated by measuring the changes in mechanical properties, crystallinity and molecular weight of polymer, water absorption, weight loss, and structural changes. Results showed that the addition of bioactive glass filler modified the degradation kinetics and material morphology.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.