Abstract

We investigated the effect of very high pressure on the sintering temperature, phase transition and the grain growth during Spark Plasma Sintering (SPS) of a 15 nm TiO 2 nanopowder. Using in situ synchrotron X-ray diffraction during sintering at 1.5 and 3.5 GPa, we followed the evolution of the crystalline phases and the crystallite size as a function of temperature. In comparison, in the laboratory, SPS experiments were performed on two original facilities: A Paris-Edinburgh press and a high-pressure module adapted to standard SPS equipment. We studied the effect of the pressure on the sintering in the range 76 MPa to 3.5 GPa. We have shown that highly dense nanostructured ceramics can be prepared under very high pressure at low sintering temperatures. At 1 GPa, we limited the grain growth to an average size of 233 nm by heating at only 560 °C, and achieved a relative density of 98%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.