Abstract

Synthesis of a novel NiAl matrix composite powder reinforced with 0–40wt.% NbB2 by combustion synthesis in thermal explosion mode was investigated. The elemental powders of Ni, Al, Nb, and amorphous boron were used as starting material. For all compositions final products consisted of only the NiAl and NbB2 phases. Coarser NbB2 with a relatively uniform distribution in NiAl matrix was formed with rising NbB2 content. Microhardness of NiAl considerably increased from 377±13 HV0.05 to 866±81 HV0.05 for NiAl with 40wt.% NbB2. High microhardness, proper size and distribution of NbB2 in NiAl matrix make it a good candidate as precursor for thermal spray application.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.