Abstract

The in situ toughened Ti–TiB ceramic–matrix composites containing high volume fraction of TiB were synthesized by spark plasma sintering technique under a pressure of 50 MPa, with sintering temperature ranging from 1100 °C to 1400 °C and heating rate of 150 °C/min, using Ti and TiB 2 powders. Results indicated that Ti–TiB composites sintered at 1400 °C provided the optimal combination of dense microstructure, well developed lath-shaped TiB grains, and excellent mechanical properties, including the relative density of 99.6%, bending strength of 608 MPa, and a rather high fracture toughness of 9.35 MPa m 1/2. Moreover, the micro-hardness of the composites reaches a relatively high level (18.3 GPa).