Abstract

A new and simple method has been proposed to prepare magnetic Fe 3O 4-chitosan (CS) nanoparticles by cross-linking with sodium tripolyphosphate (TPP), precipitation with NaOH and oxidation with O 2 in hydrochloric acid aqueous phase containing CS and Fe(OH) 2, and these magnetic CS nanoparticles were used to immobilize lipase. The effects on the sequence of adding NaOH and TPP, the reaction temperature, and the ratio of CS/Fe(OH) 2 were studied. TEM showed that the diameter of composite nanoparticles was about 80 nm, and that the magnetic Fe 3O 4 nanoparticles with a diameter of 20 nm were evenly dispersed in the CS materials. Magnetic measurement revealed that the saturated magnetisation of the Fe 3O 4-CS nanoparticles could reach 35.54 emu/g. The adsorption capacity of lipase onto nanoparticles could reach 129 mg/g; and the maximal enzyme activity was 20.02 μmol min −1 mg −1 (protein), and activity retention was as high as 55.6% at a certain loading amount.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.