Because of its exceptional qualities, aluminium composites are frequently employed in aircraft applications. Aluminium alumina composite was manufactured in-situ using the AA-6061 T6 matrix alloy and 3 %age, 6 %age (Nichrome) powder. Optical metallography, Image Analysis, and micro hardness tests were used to assess the in-situ composites. The specimens then liquid preheated at 550 °C for 3 hours and then aged at 180 °C for 7 hours to improve the durability in mechanical characteristics. In comparison to the as cast samples, the heat-treated samples showed significantly higher mechanical properties. AA-6061 T6 matrix composite reinforced with in-situ alumina particle with TiC was also studied for grain refining. The Al-4.5 % Ti-1.5 % C master alloy has been shown to be an effective grain refiner.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: European Journal of Materials Science and Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.