AbstractDirect‐ammonia proton ceramic fuel cell (DA‐PCFC) is a promising clean energy technology because ammonia (NH3) is easier to store, transport, and handle than hydrogen. However, NH3 decomposition efficiency is unsatisfactory, and the anti‐sintering resistance of conventional Ni‐based ceramic anodes has limited the large‐scale application of DA‐PCFC technology. Herein, Pr0.6Sr0.4(Co0.2Fe0.8)0.85Ru0.15O3‐δ (PSCFR15), a novel anode catalyst layer (ACL) material is developed. PSCFR15 is treated under a reducing atmosphere to form a composite with CoFeRu alloy nanoparticles. Density functional theory simulations reveal that Ru modification in the CoFe alloy promotes nitrogen desorption during ammonia decomposition reaction, thereby boosting ammonia decomposition efficiency. As a result, DA‐PCFC with PSCFR15 ACL can achieve superior peak power density compared to bare DA‐PCFC operated with H2 and NH3 fuels. Furthermore, the ACL also reduces the direct contact between the Ni‐based ceramic anode and the NH3 fuel, then suppressing Ni sintering, and enhancing the durability of the DA‐PCFC.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.