Abstract
An instrumented creep testing capability is being developed for specimens irradiated in pressurized water reactor coolant conditions at the Advanced Test Reactor (ATR). A test rig has been developed such that samples will be subjected to stresses up to 350 MPa at temperatures up to 370°C in pile. Initial Idaho National Laboratory (INL) efforts to develop this creep testing capability for the ATR are summarized. In addition to providing an overview of in-pile creep test capabilities available at other test reactors, this paper reports efforts by the INL to evaluate a prototype test rig in an autoclave at INL’s High Temperature Test Laboratory. Data from autoclave tests with Type 304 stainless steel and copper specimens are reported.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.