Abstract

The high-temperature mechanical properties and failure mechanisms of Si, BSAS and Yb2SiO5 ceramic materials are important for environmental barrier coatings. The Si coating, BSAS coating and Yb2SiO5 coating were prepared by the atmospheric plasma spray (APS) technique. The elastic modulus, fracture strength and fracture strain are determined by three-point bending combined with the digital image correlation (DIC) method. The results show that as the test temperature increases from 25 °C to 1000 °C, the elastic modulus of the Si coating and Yb2SiO5 coating decreases while the elastic modulus of the BSAS coating increases. And the fracture strength and fracture strain of the Si coating, BSAS coating and Yb2SiO5 coating increase. The elastic modulus is related to the interatomic distance and bonding strength of atoms. The fracture strength and fracture strain increase with the densification of the coating.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.