A cold working steel was coated both with high temperature CVD (TiN) and moderate temperature CVD (Ti[C,N]). AES depth profiles show a significant difference at the interface, where a thin oxide layer remains detectable at deposition temperatures of 750 °C. It could be shown that an impedance signal at a frequency of 13 MHz is well suited to detect the early stages of the growth of a CVD coating.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.