Abstract

A process based on liquid‐phase sintering and subsequent annealing for grain growth is presented to obtain in situ‐toughened SiC‐30 wt% TiC composites. Its microstructures consist of uniformly distributed elongated α‐SiC grains, matrixlike TiC grains, and yttrium aluminum garnet (YAG) as a grain boundary phase. The composites were fabricated from β‐SiC and TiC powders with the liquid forming additives of A12O3 and Y2O3 by hot pressing. During the subsequent heat treatment, the β→α phase transformation of SiC led to the in situ growth of elongated α‐SiC grains. The fracture toughness of the SiC‐30 wt% TiC composites after 6‐h annealing was 6.9 MPa‐m1/2, approximately 60% higher than that of as‐hot‐pressed composites (4.4 MPa‐m1/2). Bridging and crack deflection by the elongated α‐SiC grains appear to account for the increased toughness of this new class of composites.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.