Significant grain refinement was achieved in a cast Mg–8 mass% Li alloy through processing by equal-channel angular pressing (ECAP) using a die having an internal channel angle of 110° and a pressing temperature of 473 K. Following extrusion and subsequent ECAP through two passes, the alloy exhibited excellent superplastic properties including a maximum elongation of ∼970% at 473 K when using an initial strain rate of 1.0 × 10 −4 s −1. The strain rate sensitivities under the optimum superplastic conditions were measured as m ≈ 0.4–0.6. The maximum elongation achieved in this investigation is very high by comparison with other Mg alloys tested in tension at similar temperatures and strain rates.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.