Abstract
The transition dipole moment (TDM) orientation in the emission layer (EML) of organic light-emitting diodes (OLEDs) have attracted increasing attention from many researchers. But the study point at the molecular orientation in the hole transport layer (HTL) and electron transport layer (ETL) was not reported widely. In this paper, the molecular orientation of HTLs and ETLs were controlled by the deposition rate. The angle-dependent PL spectra and the variable angle spectroscopic ellipsometry (VASE) were used for evaluating the molecular orientation of B3PYMPM and TAPC, respectively. We found that fast deposition rate can boost preferentially vertical molecular orientation in both molecules and facilitate the hole and electron mobility, which was tested by the current density-voltage and capacitance-voltage curves of HODs and EODs. Moreover, the HTLs and ETLs were employed in OLED devices to verify the influence of molecular orientation on charge carrier mobility, which determined the performance of OLEDs significantly.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.