The technical TiAl-alloy γ-MET (Ti–46.5Al–4(Cr, Nb, Ta, B)) was oxidised thermocyclically (24 h-cycle-test) at 900 °C in wet and dry air. In this paper results of untreated and fluorine treated TiAl-samples are presented. Their oxidation behaviour will be shown. Several methods were used to apply the halogens to the surface, e.g. beamline ion implantation, spraying of or dipping into a halogen containing liquid. A pure protective alumina scale was found, e.g. after treatment with a fluorine containing polymer and thermocyclic oxidation up to 1 year at 900 °C in laboratory air. On the other side thick fast growing and non-protective mixed oxide scales were found on the untreated samples.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.