Abstract

In this study, pulse reverse current electrodeposition was employed to fabricate Fe-55 wt%Ni alloy. Abnormal grain growth induced by the precipitation of second-phase particles during annealing resulted in a coarse-grained electrodeposited Fe-55 wt%Ni alloy. The grain evolution process during annealing was investigated, and the temperature for abnormal grain growth was determined through the high-temperature confocal microscopy technique. Subsequently, the mechanism of abnormal grain growth was investigated. The results suggest that abnormal grain growth occurs at approximately 1003 K, attributed to the preferential growth of (110) oriented grains due to local strain energy changes caused by the precipitation and coarsening of the second-phase particles (MnS). The preferred orientation of the grains transitioned from (111) to (110). Annealing at 1073 K for 2 h resulted in an average grain size increase to approximately 200 μm. Under these conditions, the magnetic properties of the alloy reached optimal levels, with a magnetization saturation strength of 186.7 emu g−1 and a coercivity of less than 1 Oe. This research presents a novel approach to preparing coarse-grained electrodeposited Fe-Ni alloys, significantly enhancing their magnetic properties.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.