Abstract
A widely used oxyanion corrosion inhibitor (Li2CrO4) was used as electrolyte additive (3.5 wt% NaCl solution was used as electrolyte solution) for Mg–air battery. The potentiodynamic polarization tests showed that the presence of 0.1 wt% Li2CrO4 in the NaCl electrolyte reduced enormously the corrosion current density of the tested AZ31 Mg alloys. According to the intermittent discharge tests, the use of 0.1 wt% Li2CrO4 as electrolyte additive increased the anode efficiency of the Mg–air battery by 28.4%. The addition of 0.1 wt% Li2CrO4 reduced the anode self-corrosion rate of the battery in the intermittent stage effectively. The product film after discharge was observed by scanning electron microscope, and the Mg–air battery containing 0.1 wt% Li2CrO4 has a loose product film, which is beneficial to its discharge performance. So using Li2CrO4 as electrolyte additive could improve the intermittent discharge performance of Mg–air battery. And the use of oxyanion corrosion inhibitor as electrolyte additive may be an excellent way to improve the intermittent discharge performance of Mg–air battery.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.