Abstract

Chitosan (CS) was grafted with 0.1 and 0.5% (w/v) palmitic acid (PA) to improve its encapsulation efficiency (EE) and sustained release characteristics when forming CS microparticles. Thereafter, PA-grafted CS (PA-CS) microparticles were coated with denatured β-lactoglobulin (βlg), which forms an outer protective layer. The possibility of hydrophobic interaction with the hydrophobic substances in the CS microparticles increased as the proportion of the grafted PA increased. EE was measured as 64.79, 83.72, and 85.00% for the non-grafted, 0.1, and 0.5% PA-CS microparticles, respectively. In simulated small intestinal conditions, 4.66 and 17.55% of the core material release in the PA-CS microparticles were sustained after 180min by 0.1, and 0.5% PA grafting, respectively. PA grafting enables the sustained release in simulated gastrointestinal fluids by enhancing the hydrophobic interaction between CS and the hydrophobic core material.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call