Abstract
Open-cell Inconel 625 superalloy foams were prepared by suspension impregnation method which involves replication of pure nickel foam ligaments with a mixed powder suspension and subsequent heat treatments. The objective of the present study is to find a suitable method ensuring complete densification of the superalloy foam ligaments without using low-melting additives and achieving uniform chemical composition at moderate sintering temperatures. Foams prepared using the above methodology were evaluated for the microstructure and compositional variation across the foam ligaments by scanning electron microscopy (SEM) coupled with electron dispersive spectroscopy (EDS). Quasi-static compressive properties of the foams were evaluated. It is shown that if elemental powders of Cr, Mo and Ni are used as additives to the superalloy powder suspension, high ligament density with uniform chemical composition conforming to the Inconel 625 specification is achieved at moderate sintering temperatures. These results are attributed to the formation of low melting eutectics and to acceleration of the diffusion kinetics due to the non-equilibrium thermodynamic conditions created by large compositional gradients in the presence of elemental powders.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Transactions of Nonferrous Metals Society of China
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.