This study was carried out to determine the possibility of reducing the iron oxide ratio in silica sand from Ardhumah, an area, (18) km west of Rutba, a city in Al-Anbar Governorate, to obtain sand specifications appropriate for making colorless glasses (not exceeding 0.02 % iron oxide ratio). The reduction process of iron oxide includes three stages; the first stage is magnetic separation to reduce Fe2O3 from 0.092% to 0.040%, the second stage is re-floatation which has reduced Fe2O3 to 0.024%, finally treatment of the sand output from the first and second stage with diluted HCl or H2SO4, this study showed the possibility of obtaining silica sand with a ratio of Fe2O3 up to 0.016%.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.