Abstract

Hook defect (HD) seriously decreases the mechanical properties of friction stir spot welded (FSSW) joints. In this study, two methods were therefore used to eliminate the HD in pinless FSSW joints. The one is changing welding parameters such as rotating speed and dwell time. The other one is FSSW plus subsequent friction stir welding (FSSW-FSW), which is an innovative method proposed in this study. Experimental results showed that the HD in pinless FSSWed AA2024 joints was successfully eliminated by using FSSW-FSW, not by changing process parameters. The joints without HD exhibited a tensile–shear load of as much as 12kN, which was higher than that of 6.9kN in the joints with HD. Furthermore, it was proved that the tensile–shear load is not greatly improved only by increasing the nugget zone when HD still existed in the FSSW joints. In addition, the fracture morphology analysis demonstrated that the shear fracture of the FSSW-FSW joints took place along the boundary between the upper and lower sheets through the weld nugget, and the faying surface between the two sheets was completely sheared off.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call