Abstract
To increase the lap shear failure load of friction stir lap welding (FSLW) joint, a tool with a bottom-half-threaded pin was designed in the present study. Using 7N01-T4 aluminum alloy as the research object, tools with the bottom-half-threaded pin and the traditional full-threaded pin were used to fabricate lap joints. Results showed that the thread end position on the pin greatly influenced the material flow behavior. The material concentrated zone using the bottom-half-threaded pin mainly located above the lap interface, which is beneficial to suppress the hook and cold lap. The lap shear failure load of the FSLW joint using the bottom-half-threaded pin was 17,644.7 N, which is equal to 122.8 % of the joint using the full-threaded pin.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: The International Journal of Advanced Manufacturing Technology
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.