Abstract
The a-IGZO deposited by using the rf sputtering method features a conductive or an insulator characteristic based on amount of oxygen. We demonstrated that a post-treatment affects the resistance patterns of particular-sized InGaZnO(IGZO) thin films in a-IGZO thin-film transistors (TFTs). Post-annealing shifted the driving voltage of a-IGZO TFT to positive or negative values, depending on the annealing temperatures. Post-annealing may introduce oxygen vacancies or desorbed oxygen in the IGZO thin film. The changed driving voltage of IGZO TFTs coincides with the shift of the resistance pattern of IGZO. The fabricated a-IGZO TFTs exhibited a field effect mobility of 6.2 cm2/Vs, an excellent subthreshold gate swing of 0.32 V/decade, and a high I on/off ratio of > 109. Under positive bias illumination stress (PBIS) and negative bias illumination stress (NBIS), after 3,600 seconds, the device threshold voltage shifted about 0.2 V and 0.3 V, respectively.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.