Abstract

Niobium-doped Pb(Zr0.53Ti0.47)O3 (PZTN) ceramics were prepared by the conventional(mixed oxides) method, modified by the addition of a PZT colloid of the same composition. The colloidal precursor was prepared using a coprecipitation method. Such an addition produced a significant improvement in the sinterability of a conventionally prepared PZTN powder and the sintering temperature was reduced, achieving a density ⩾98% theoretical density at 1075 °C for 2 h. The measured piezoelectric properties were as high askp = 0.62 andd33 = 330 ×10−12CN−1.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.