Abstract

Addition of Fe refines the microstructure of Mo76-xSi14B10Fex (x = 0, 0.5, 1 at.%) composites containing α-Mo, Mo3Si and Mo5SiB2 phases, increases the hardness from 950 Hv (x = 0) to 1031 Hv (x = 1), and improves the oxidation resistance at temperature in the range of 800–1300 °C. The hardness of the base alloy substrate decreases only by <7% than that of as-solidified ingots, indicating good microstructural stability of the composite for high temperature application.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.