Abstract

Pure and CdsNi(NP) were prepared by thermal deposition. The influence of the Ni doping ratio has studied these films' structural, morphological, optical, and electrical properties. Polycrystalline hexagonal (CdS and CdSNi) were shown to have [101] preferential orientation by XRD analysis. Images from the (FE-SEM) showed low-dimension NP formation, and the NP size was in the region of 15–25 nm. Optical analysis has shown that all the films are really transparent. In the visible region, the transmittance ranges between 75% and 80%, were based on the concentration of the dopant. The film with a Ni ratio of 0.3 % showed a minimum resistivity of 6.14x105 Ω.cm at RT.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.