Abstract

Silver (Ag) electrodes are prepared by an electrodeposition method at −0.25 V versus SCE. To evaluate the effect of particle size on Li–air cells, deposition times are 3, 10, 30, and 300 s. When cycled at a current density of 0.032 mA cm–2, the Ag-deposited electrode for 300 s shows very low polarization corresponding to the oxygen evolution reaction potential at 3.6 V. X-ray diffraction studies confirm that the main discharge product is Li2O2, and the results of scanning electron microscopy and transmission electron microscopy of the discharged electrodes show lithium peroxides at different positions due to the limitation of active sites on silver particles.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.