Abstract

(Ba 0.6Sr 0.4)(Ti 1− x Zr x )O 3 (0.05 ≤ x ≤ 0.3) ferroelectric materials have cubic perovskite structure and show paraelectric properties at room temperature. Curie point shifted to a negative value as increasing Zr content in (Ba 0.6Sr 0.4)(Ti 1− x Zr x )O 3 system. When Zr substituted 0.1 mol, the dielectric constant, dielectric loss, tunability, Curie point and FOM were 4500, 0.0005, 63%, −1.6 °C and 1260, respectively. This composition shows excellent microwave dielectric properties than those of (Ba 0.6Sr 0.4)TiO 3 ferroelectrics, which are limelight materials for tunable devices such as varactors, phase shifters and frequency agile filters, etc.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.