Abstract

Various oxide dispersion strengthened (ODS) steels which have high Cr concentrations with and without Al addition were made by mechanical alloying method. Corrosion measurement was done in the closed system of super critical pressurized water (SCPW) at 783 K with the pressure of 25 MPa. In order to evaluate the mechanical properties and the effect of thermal aging, a miniaturized Charpy V notch (MCVN) test and tensile test were performed before and after aging at 773 K up to 1000 h. The susceptibility to stress corrosion cracking (SCC) of high Cr-ODS steels was evaluated by slow strain rate test (SSRT). The SSRT was performed in a simulated boiling water reactor (BWR) condition with high temperature oxygenated (8–10 ppm) water at 561 K and at a pressure of 7.8 MPa. Strain rates were ranging from 1 × 10 −4 to 3 × 10 −7 s −1. The high Cr-ODS steels showed a better resistance to corrosion than SUS316L stainless steel in SCPW. The 14Cr and 16Cr-ODS steel did not suffer from aging embrittlement at 773 K for 1000 h. The ODS steels showed no susceptibility to SCC at strain rates from 1 × 10 −4 to 3 × 10 −7 s −1.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.