Abstract

Gadolinium zirconate (Gd2Zr2O7, GZ) as one of the promising thermal barrier coating materials for high-temperature application in gas turbine was toughened by nanostructured 3mol% yttria partially-stabilized zirconia (YSZ) incorporation. The fracture toughness of the composite of 90mol% GZ-10mol% YSZ (GZ–YSZ) was increased by about 60% relative to the monolithic GZ. Both the GZ and GZ–YSZ composite coatings were deposited by atmospheric plasma spraying on Ni-base superalloys and then thermal-shock tested under the same conditions. The thermal-shock lifetime of GZ–YSZ composite coating was improved, which is believed to be mainly attributed to the enhancement of fracture toughness by the addition of YSZ. In addition, the failure mechanisms of the thermal-shock tested GZ–YSZ composite coatings were discussed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.