Silica is the most reinforcing filler for enhancing the rubber properties. However, the incompatibility of silica with non-polar rubber is the main problem for application. Therefore, the researchers attempted to use the several methods in order to solve the problem. In this work, the appropriated hydroxyl telechelic natural rubber (HTNR) was determined by varying molecular weights in the range of 2,000-3,000 g·mol-1 and contents in the range of 4-16%w/w of silica content in order to enhance the rubber properties. It was found that the decrease in Payne effect and the improvement in cure characteristics of silica-reinforced NR were achieved by using HTNR. However, the incorporation of various molecular weights and contents of HTNR in rubber influenced C1 (crosslink density determined by stress-strain measurement) in rubber, which related to rubber properties. The increasing in C1 caused the increases in tensile strength and abrasion index and the decrease in heat build-up. The optimum properties of rubber with silica loading at 30 phr was achieved by adding 2,000 g·mol-1 HTNR at a loading of 8%w/w of silica content. However, for silica-reinforced NR, TESPT provided better properties than HTNRs.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.