Abstract

The average plastic strain ratio (the R-value) and the anisotropy parameter |ΔR| calculated from the measured texture of AA1050 Al alloy sheet treated by the heavy asymmetric rolling by 84% reduction in thickness and subsequent annealing for 1 h at 500 °C, followed by light rolling by 10% or 20% reduction in thickness and the subsequent annealing for 1 h at 500 °C increased by 1.52 times that of the non-processed specimen and reduced to 1/12 times that of the non-processed specimen, respectively.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.