The broad applications of 3D-printed poly-ether-ether-ketone (3D-PEEK) structures are largely hampered by their inadequate mechanical properties that can be improved by post treatments. At present, thermal annealing is generally used to improve the mechanical properties of 3D-PEEK. However, it cannot simultaneously improve strength and ductility. Here, a cost-effective postprocessing method is developed to improve the mechanical properties of 3D-PEEK, based on annealing in nonsolvent vapor at room temperature. The annealing in nonsolvent vapor at room temperature simultaneously improves the strength, ductility, and fracture energy of as-printed 3D-PEEK by 22.6%, 151.3%, and 109.1%, respectively. The improved mechanical properties are attributed to enhanced interfacial bonding, increased crystallinity, decreased pinhole defects, and stress relaxation in the 3D-PEEK. Moreover, the annealing in both polar solvents (such as acetone and chloroform) and nonpolar solvents (such as n-hexane) are demonstrated to be effective for improving the mechanical properties of 3D-PEEK. The nonsolvent vapor-annealed 3D-PEEK can thus have potential applications in the fields of medical implants, automotive, aerospace, and more.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.