Abstract

Research is conducted within the scope of the Clean Steel project into reasons for variation of the metal level in a crystallizer and breakouts of the crystallizing metal skin in a thin-slab CCM, and also a study of reasons for defect formation in hot-rolled strip. Examples are provided of improved monitoring and control of the VMZ casting and rolling complex (CRC) technology. Implementation of the monitoring production technology – evaluation of metal product quality – operational adjustment of technology concept makes it possible to reduce the CCM emergency situation index to less than 0.5 ton/105 tons of steel, and also to determine factors influencing the formation of transverse cracks over a rolling mark, and to remove defect formation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.