We examined the surface modifications of Zr50Cu30Ni10Al10 bulk glassy alloys, including oxidization, nitriding, and diamond-like carbon (DLC) coating to improve wear resistance. Wear abrasion in bulk glassy alloys begins with the formation of shear bands, as in cold-rolled structures. Ultimately, lamellar tearing occurs in the lamellar structure of the shear band in the wear region. Surface modification effectively reduces the wear abrasion corresponding to the easy formation of the shear band. Bulk glassy alloy coated with DLC has outstanding wear resistance due to its low surface-friction coefficient. [doi:10.2320/matertrans.47.1999]

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.