Abstract

To improve thermoelectric performance, polar-solvent vapor annealing (PSVA) method was introduced into the preparation of poly(3,4-ethylenedioxythiophene):poly(styrene sulfonate) (PEDOT:PSS) films. The solvent vapors included dimethyl sulfoxide, ethylene glycol, N,N-dimethylformamide, N-methyl-2-pyrrolidone, and deionized water (H2O). The PSVA-treated PEDOT:PSS films exhibited significantly enhanced electrical conductivity and the maximum value was up to 496 S cm−1. Especially, utilizing the PSVA method, H2O could also remarkably enhance the electrical conductivity of pristine PEDOT:PSS film from 0.2 to 57 S cm−1. There was no distinct change for the Seebeck coefficient of PSVA-treated films with the significantly enhanced electrical conductivity, thereby a maximum power factor of 9.47 μW m−1 K−2 at room temperature was obtained. The effects of PSVA method on thermoelectric performance of PEDOT:PSS films were also investigated systematically by analyzing the changes in morphology, carrier mobility and carrier concentration. The results confirmed that PSVA-treated PEDOT:PSS films could obtain smoother morphologies and realize the simultaneous increase of carrier mobility and carrier concentration, which results in the improvement of the thermoelectric performance.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.