Abstract

Improvement of the thermal stability of continuous SiC fiber reinforced SiC ceramic matrix composites (SiCf/SiC CMC) by the pre-treatment of SiC fillers and the suppression of oxidation during polymer impregnation and pyrolysis (PIP) process were investigated. Dense SiCf/SiC CMCs were fabricated using the slurry infiltration and PIP process under a purified argon atmosphere. Structure and mechanical properties of the SiCf/SiC CMC heated at different temperatures were evaluated. The flexural strength of the SiCf/SiC CMC decreased only 15.3%after heating at 1400 ?C, which exhibited a clear improvement compared with the literature data (49.5% loss), where severe thermal deterioration of SiCf/SiC composite occurred at high temperatures by the crystallization and decomposition of the precursor-derived ceramic matrix. The thermal stability of the SiCf/SiC CMC fabricated by PIP process was improved by the pre-treatment of SiC fillers for removing oxides and the strict atmosphere control to prevent oxidation.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.