Abstract

A significant source of copper losses from pyrometallurgical copper extraction is attributed to dissolved and entrained copper in discarded slag. Entrained copper can be recovered via pyrometallurgical slag cleaning in a settling furnace, where the slag viscosity and copper droplet size distribution (CDSD) are critical parameters. Reduced copper losses suggest improved raw material efficiency, and the slag becomes a more environmentally safe byproduct. In this study, iron silicate slags from a smelting furnace are industrially CaO modified in a fuming furnace to contain a CaO content between 8 and 18 wt.%. The viscosity of slags with and without CaO modifications is evaluated in the temperature range from 1423 to 1723 K. The influences of the CaO modifications on the CDSD, slag matrix copper content, and total copper content were determined. The results show that the slag viscosity decreases with increasing CaO concentrations in the slag. In addition, the copper content decreases in the slag phase, and the CDSD shifts to contain relatively larger droplets. The effect of CaO slag modification reveals a linear relationship between the overall copper recovery and viscosity, which increased from 63 to 88% when the viscosity in the respective batch was 0.51 and 0.25 Pa·s.Graphical

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call