Abstract
Dy-Co-modified aluminide coating was deposited onto Ni-based superalloy DZ125 using pack cementation method. The microstructure and hot corrosion behavior of the coating were investigated. The results show that as-deposited coating has a two-layer structure. The outer layer of the coating is composed mainly of Al0.9Ni1.1 with dispersed Dy2Hf2O7. The mass gain of the coating is 0.23mg/cm2 after exposure to 75wt.% Na2SO4+25wt.% NaCl at 900°C for 100h. The corrosion product formed on the coating is characterized as Al2O3. Role of Dy in the improvement of the hot corrosion resistance has been discussed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.