Zirconium substituted 0.8BaTiO3-0.2Bi0.5K0.5TiO3 lead free ceramic materials were prepared by solid state reaction followed by high energy ball milling process. To understand its frequency dependent electrical properties, impedance spectroscopic studies were carried out. From the impedance studies it is observed that relaxation taken place from 375 °C. Single depressed semicircle was observed from the Cole-Cole plots. This indicates non-Debye kind of relaxation process. Grain resistance value was calculated from the Cole-Cole plots and it is found to be increasing with increase of Zr substitution. Modulus spectroscopic studies also confirm the non-Debye kind of relaxation process in the material. Variations in normalized values of / max & / max as a function of logarithm of frequency indicates short range conductivity in the present material.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.