Abstract

Porous ZnO/dye hybrid films have been deposited by cathodic electrodeposition, and their active surface area after dye desorption was evaluated by impedance measurements with the semiconducting electrode polarized in accumulation. Surface area ratios have been deduced for a large number of films from imaginary part Z″ vs. frequency measurements, having a constant rate over the frequency range from 0.5 Hz to > 50 Hz. The active surface increased by a factor of roughly 150 per every micron of film with respect to the area of a flat ZnO electrode: this linear relationship held from less than 1 µm up to 9 µm thick films.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.