Abstract

Landfill leachate is generally transferred to in situ facilities for advanced treatmentby using a pipe system. Because of its harmful and complex compounds, leachate may react with pipe materials, leading to corrosion and scaling. This experimental study uses typical PVC pipe material and investigates its anti-corrosion performance by placing the material samples into different aged leachates. By evaluating the changes in different experimental parameters, including calcium, magnesium, and chloride ion concentration, oxidation-reduction potential, dissolved oxygen, and pH, combined with a characterization of the material properties, we infer the main causes of pipe scaling-corrosion. Results show that the scaling is more intense in the younger leachate, and the concentration of calcium ions is the dominant influencing factor. The scaling might be resulted from joint actions of chemical precipitation and microbial metabolic activities. It is expectedthe study to provide useful insights into taking effective actions on anti-clogging, and enhance pipes design by selection of appropriate materials for future modification.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.