Abstract

When particleboards are exposed to water or moist environment, they tend to swell and expand in all directions. The degree of swelling or expansion depends on the type of adhesive used, its share, and the time of exposure and pressure used at hot pressing. The expansion of particleboard, exposed to water or high moisture content, is accompanied by swelling and/or expansion pressure. The purpose of this paper is to present the impact of adhesive share on thickness swelling and swelling pressure of three layer particleboard bonded with urea-formaldehyde adhesive. The resin content was altered in both layers ; in core layer it was between 6 and 9 %, and in surface layer between 11 and 13 %. Thickness swelling and swelling pressure were determined with 24-hour immersion lest. For the swelling pressure measurement, special force gauge device was used. The biggest changes in swelling and pressure were observed when the resin content was changed in core layer The fastest change in swelling and swelling pressure was observed in the, first few hours after immersion in water.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.