Abstract

This work deals with emphasizing the relation between particle dimension distribution of nanocellulose (PDD) particles with its efficiency as stabilizing/adsorbent agent of Indigo dye. In this respect, different pulping reagents were used in preparation of Rice straw pulps as precursors for nanocelluloses using acid hydrolysis and oxidizing agents [(KMnO4 and NH4)2S2O8] methods. The PDD was estimated by indirect method through processing the TEM images using the software ImageJ. The resulting nanocelluloses were also characterized by X-ray diffraction (XRD) and Fourier-transform infrared spectra (FTIR) together with sulfate ester and carboxyl contents. The data showed the effective role of pulping reagent on PDD. The cellulose nanocrystals (CNCs) from NaOH-AQ pulp, with the longest crystal length (204.4 ± 107.8 nm) and the lowest diameter (6.7 ± 2.3 nm), exhibited most stabilized suspension of dye; however, the highest adsorption capacity was accompanied the oxidized nanocellulose (Ox-NC) from neutral RS pulp with lowest PDD (4.98 ± 1.6 and 90.5 ± 3.14), together with highest COO content (476.46 μmol/g).

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call